DESCRIPTION
ISO 15609-6:2013
ISO 15609-6:2013 specifies requirements for the content of welding procedure specifications for laser-arc hybrid welding processes. Variables listed in ISO 15609-6:2013 are those influencing the quality and the properties of the welded joint.