PRICES include / exclude VAT
Homepage>CSN Standards>42 METALLURGY>4203 Mechanical testing of metals>CSN EN ISO 204 - Metallic materials - Uniaxial creep testing in tension - Method of test
FREE SHIPPINGReleased: 2018
CSN EN ISO 204 - Metallic materials - Uniaxial creep testing in tension - Method of test

CSN EN ISO 204

Metallic materials - Uniaxial creep testing in tension - Method of test

CURRENCY
LANGUAGE
English
Category:420351
Released:2018
Number of Standard:CSN EN ISO 204
DESCRIPTION

EN ISO 204


EN ISO 204 Metallic materials - Uniaxial creep testing in tension - Method of test -

Original English text of CSN EN Standard.
The price of the Standard included all amendments and correcturs.
Related products
FREE SHIPPING
Released: 2016
CSN EN 10314
Method for the derivation of minimum values of proof strength of steel at elevated temperatures
LANGUAGE
English
FREE SHIPPING
Released: 2017
CSN EN ISO 377
Steel and steel products - Location and preparation of samples and test pieces for mechanical testing
LANGUAGE
English