ISO 7539-10 Corrosion of metals and alloys — Stress corrosion testing — Part 10: Reverse U-bend method

ISO 7539-10

Corrosion of metals and alloys — Stress corrosion testing — Part 10: Reverse U-bend method

Format
Availability
Price and Currency
English PDF
Immediate download
103.53 USD
English Hardcopy
In stock
103.53 USD
French PDF
Immediate download
103.53 USD
French Hardcopy
In stock
103.53 USD
Standard´s number:ISO 7539-10
Pages:15
Edition:2
Released:2020
DESCRIPTION

ISO 7539-10


This document specifies procedures for designing, preparing and using reversed U-bend (RUB) test specimens for investigating the susceptibility of the metal to stress corrosion cracking. The term "metal" as used in this document includes alloys.