UNE EN ISO 25239-4:2012
Friction stir welding - Aluminium - Part 4: Specification and qualification of welding procedures (ISO 25239-4:2011)
Soldeo por fricción-agitación. Aluminio. Parte 4: Especificación y cualificación de los procedimientos de soldeo. (ISO 25239-4:2011).
CURRENCY
Standard number: | UNE EN ISO 25239-4:2012 |
Pages: | 32 |
Released: | 2012-11-07 |
DESCRIPTION
This standard UNE EN ISO 25239-4:2012 Friction stir welding - Aluminium - Part 4: Specification and qualification of welding procedures (ISO 25239-4:2011) is classified in these ICS categories:
- 25.160.01
- 25.160.10
- 25.160.40