Don't have a credit card? Never mind we support BANK TRANSFER .

PRICES include / exclude VAT
Homepage>ASTM Standards>17>17.200>17.200.10>ASTM E1952-23 - Standard Test Method for Thermal Conductivity and Thermal Diffusivity by Modulated Temperature Differential Scanning Calorimetry
Released: 01.06.2023

ASTM E1952-23

Standard Test Method for Thermal Conductivity and Thermal Diffusivity by Modulated Temperature Differential Scanning Calorimetry

Format
Availability
Price and currency
English PDF Redline
Immediate download
70.55 EUR
English PDF
Immediate download
58.65 EUR
English Hardcopy
In stock
58.65 EUR
Standard number:ASTM E1952-23
Released:01.06.2023
Status:Active
Pages:7
Section:14.01
Keywords:ceramics; differential scanning calorimetry (DSC); glasses; modulated differential scanning calorimetry (MDSC); modulated temperature differential scanning calorimetry; polymers; thermal analysis; thermal conductivity; thermal diffusivity;
DESCRIPTION

1.1 This test method describes the determination of thermal conductivity of homogeneous, non-porous solid materials in the range of 0.10 W/(K·m) to 1.0 W/(K·m) by modulated temperature differential scanning calorimeter. This range includes many polymeric, glass, and ceramic materials. Thermal diffusivity, which is related to thermal conductivity through specific heat capacity and density, may also be derived. Thermal conductivity and diffusivity can be determined at one or more temperatures over the range of 0 °C to 90 °C.

1.2 The values stated in SI units are to be regarded as standard.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.