BS 4870-2:1982
Specification for approval testing of welding procedures TIG or MIG welding of aluminium and its alloys
CURRENCY
| Standard number: | BS 4870-2:1982 |
| Pages: | 20 |
| Released: | 1982-02-26 |
| ISBN: | 0 580 12562 9 |
| Status: | Standard |
DESCRIPTION
BS 4870-2:1982
This standard BS 4870-2:1982 Specification for approval testing of welding procedures is classified in these ICS categories:
- 25.160.01 Welding, brazing and soldering in general
Items to be recorded in welding procedure tests, changes affecting approval, extent of approval, types of test weld, non-destructive and destructive testing, statement of results, recommended procedure test record form.