ISO 14001:2026 - Environmental management systems — Requirements with guidance for use - Order now!

PRICES include / exclude VAT
>BSI Standards >25 MANUFACTURING ENGINEERING>25.160 Welding, brazing and soldering>25.160.01 Welding, brazing and soldering in general>BS 4872-2:1976 Specification for approval testing of welders when welding procedure approval is not required TIG or MIG welding of aluminium and its alloys
immediate downloadReleased: 1976-04-30
BS 4872-2:1976 Specification for approval testing of welders when welding procedure approval is not required TIG or MIG welding of aluminium and its alloys

BS 4872-2:1976

Specification for approval testing of welders when welding procedure approval is not required TIG or MIG welding of aluminium and its alloys

Format
Availability
Price and currency
English Secure PDF
Immediate download
Printable - You are authorized to print 1 copy
311.15 USD
English Hardcopy
In stock
311.15 USD
Standard number:BS 4872-2:1976
Pages:26
Released:1976-04-30
ISBN:0 580 08599 6
Status:Standard
DESCRIPTION

BS 4872-2:1976


This standard BS 4872-2:1976 Specification for approval testing of welders when welding procedure approval is not required is classified in these ICS categories:
  • 25.160.01 Welding, brazing and soldering in general

This British Standard specifies requirements for the approval testing of welders to be engaged on the TIG or MIG welding of those aluminium and aluminium alloy fabrications for which the welding procedure itself does not have to be approved.

NOTE This link to the non-mandatory approval of the welding procedure will result in the use of this standard becoming defined more closely in respect of the particular fabrication, e.g. with regard to material, thickness and joint configuration.


Choice of 12 test welds covering sheet, plate and pipe, with requirements for examination and testing.