PRICES include / exclude VAT
>BSI Standards >77 METALLURGY>77.060 Corrosion of metals>BS EN ISO 15324:2008 Corrosion of metals and alloys. Evaluation of stress corrosion cracking by the drop evaporation test
immediate downloadReleased: 2008-06-30
BS EN ISO 15324:2008 Corrosion of metals and alloys. Evaluation of stress corrosion cracking by the drop evaporation test

BS EN ISO 15324:2008

Corrosion of metals and alloys. Evaluation of stress corrosion cracking by the drop evaporation test

Format
Availability
Price and currency
English Secure PDF
Immediate download
Printable - You are authorized to print 1 copy
185.92 EUR
English Hardcopy
In stock
185.92 EUR
Standard number:BS EN ISO 15324:2008
Pages:14
Released:2008-06-30
ISBN:978 0 580 60538 3
Status:Standard
DESCRIPTION

BS EN ISO 15324:2008


This standard BS EN ISO 15324:2008 Corrosion of metals and alloys. Evaluation of stress corrosion cracking by the drop evaporation test is classified in these ICS categories:
  • 77.060 Corrosion of metals