PRICES include / exclude VAT
>BSI Standards >77 METALLURGY>77.060 Corrosion of metals>BS EN ISO 7539-5:1995 Corrosion of metals and alloys. Stress corrosion testing Method for the preparation and use of C-ring specimens
immediate downloadReleased: 1995-09-01
BS EN ISO 7539-5:1995 Corrosion of metals and alloys. Stress corrosion testing Method for the preparation and use of C-ring specimens

BS EN ISO 7539-5:1995

Corrosion of metals and alloys. Stress corrosion testing Method for the preparation and use of C-ring specimens

Format
Availability
Price and currency
English Secure PDF
Immediate download
Printable - You are authorized to print 1 copy
185.92 EUR
English Hardcopy
In stock
185.92 EUR
Standard number:BS EN ISO 7539-5:1995
Pages:18
Released:1995-09-01
ISBN:0 580 18795 0
Status:Standard
DESCRIPTION

BS EN ISO 7539-5:1995


This standard BS EN ISO 7539-5:1995 Corrosion of metals and alloys. Stress corrosion testing is classified in these ICS categories:
  • 77.060 Corrosion of metals

Procedures for designing, preparing and using C-ring test specimens for investigating the susceptibility of a metal to stress corrosion.