BS EN ISO 7539-7:2005 Corrosion of metals and alloys. Stress corrosion testing Method for slow strain rate testing

BS EN ISO 7539-7:2005

Corrosion of metals and alloys. Stress corrosion testing Method for slow strain rate testing

Format
Availability
Price and currency
English Secure PDF
Immediate download
Printable - You are authorized to print 1 copy
185.92 EUR
English Hardcopy
In stock
185.92 EUR
Standard number:BS EN ISO 7539-7:2005
Pages:16
Released:2005-02-21
ISBN:0 580 45476 2
Status:Standard
DESCRIPTION

BS EN ISO 7539-7:2005


This standard BS EN ISO 7539-7:2005 Corrosion of metals and alloys. Stress corrosion testing is classified in these ICS categories:
  • 77.060 Corrosion of metals

This part of ISO 7539 covers procedures for conducting slow strain rate tests for investigating susceptibility of a metal to stress corrosion cracking, including hydrogen-induced failure.

The term “metal” as used in this part of ISO 7539 includes alloys.

Slow strain rate tests are adaptable for testing a wide variety of product forms, including plate, rod, wire, sheet and tubes, as well as composites of these and parts joined by welding. Notched specimens may be used, as well as initially plain specimens.

The principal advantage of the test is the rapidity with which susceptibility to stress corrosion cracking of a particular metal/environment combination can be assessed.