BS EN ISO 7539-9:2021 - TC Tracked Changes. Corrosion of metals and alloys. Stress corrosion testing Preparation and use of pre-cracked specimens for tests under rising load or rising displacement

BS EN ISO 7539-9:2021 - TC

Tracked Changes. Corrosion of metals and alloys. Stress corrosion testing Preparation and use of pre-cracked specimens for tests under rising load or rising displacement

Format
Availability
Price and currency
English Secure PDF
Immediate download
Printable - You are authorized to print 1 copy
427.84 EUR
English Hardcopy
In stock
427.84 EUR
Standard number:BS EN ISO 7539-9:2021 - TC
Pages:90
Released:2021-09-30
ISBN:978 0 539 20340 0
Status:Tracked Changes
DESCRIPTION

BS EN ISO 7539-9:2021 - TC


This standard BS EN ISO 7539-9:2021 - TC Tracked Changes. Corrosion of metals and alloys. Stress corrosion testing is classified in these ICS categories:
  • 77.060 Corrosion of metals