DIN EN ISO 17781
Petroleum, petrochemical and natural gas industries - Test methods for quality control of microstructure of ferritic/austenitic (duplex) stainless steels (ISO 17781:2017); English version EN ISO 17781:2017
Erdöl-, petrochemische und Erdgasindustrie - Prüfverfahren für die Qualitätslenkung von Mikrostrukturen von ferritisch/austenitisch nichtrostenden Duplexstählen (ISO 17781:2017); Englische Fassung EN ISO 17781:2017
Format
Availability
Price and currency
English PDF
Immediate download
Printable
131.44 USD
English Hardcopy
In stock
131.44 USD
German PDF
Immediate download
Printable
131.44 USD
German Hardcopy
In stock
131.44 USD
| Status: | Standard |
| Released: | 2017-11 |
| Standard number: | DIN EN ISO 17781 |
| Name: | Petroleum, petrochemical and natural gas industries - Test methods for quality control of microstructure of ferritic/austenitic (duplex) stainless steels (ISO 17781:2017); English version EN ISO 17781:2017 |
| Pages: | 30 |