ISO 15324:2000-Corrosion of metals and alloys — Evaluation of stress corrosion cracking by the drop evaporation test

ISO 15324:2000

ISO 15324:2000-Corrosion of metals and alloys — Evaluation of stress corrosion cracking by the drop evaporation test

Format
Availability
Price and currency
English PDF
Immediate download
Printable
74.00 EUR
English Hardcopy
In stock
74.00 EUR
French PDF
Immediate download
Printable
74.00 EUR
French Hardcopy
In stock
74.00 EUR
Standard´s number:ISO 15324:2000
Pages:9
Edition:1
Released:2000
DESCRIPTION

ISO 15324:2000


1.1 This International Standard specifies the procedure for determining the relative resistance of stainless steels and nickel-base alloys to stress corrosion cracking in a sodium chloride drop evaporation system. 1.2 The method results in a threshold stress to fracture, the magnitude of which can be used to rank the relative performance of different alloys for this environment.