PRICES include / exclude VAT
immediate downloadReleased: 2024-09-30
ISO 22206:2024
ISO 22206:2024 - Kraft lignin — Glass transition temperature by differential scanning calorimetry
Format
Availability
Price and currency
English PDF
Immediate download
Printable
72.36 EUR
English Hardcopy
In stock
72.36 EUR
French PDF
Immediate download
Printable
72.36 EUR
French Hardcopy
In stock
72.36 EUR
| Standard´s number: | ISO 22206:2024 |
| Edition: | 1 |
| Released: | 2024-09-30 |
| Pages (English): | 7 |
| Pages (French): | 7 |
DESCRIPTION
ISO 22206:2024
This document describes a method for the determination of the glass transition temperature (Tg) of kraft lignin. The procedure utilizes differential scanning calorimetry (DSC).
This procedure is applicable to solid lignins (e.g., powdered form) isolated using different isolation techniques (e.g., acidification with hydrochloric acid, sulfuric acid, etc., and carbonation using gaseous carbon dioxide) from the spent liquor (black liquor) generated from the kraft pulping process.
It does not apply to raw black liquor and lignin in the alkali form, (lignin that is separated from wood chips and dissolved in sodium sulfide and sodium hydroxide liquor such as that originating from black liquor).