ISO 24087:2023-Rubber, vulcanized — Determination of the glass transition temperature and enthalpy by differential scanning calorimetry

ISO 24087:2023

ISO 24087:2023-Rubber, vulcanized — Determination of the glass transition temperature and enthalpy by differential scanning calorimetry

Format
Availability
Price and currency
English PDF
Immediate download
Printable
118.00 EUR
English Hardcopy
In stock
118.00 EUR
French PDF
Immediate download
Printable
118.00 EUR
French Hardcopy
In stock
118.00 EUR
Standard´s number:ISO 24087:2023
Pages:13
Edition:1
Released:2023
DESCRIPTION

ISO 24087:2023


This document specifies a method of thermal analysis of vulcanized rubber by differential scanning calorimetry (DSC). This method is intended for the observation and measurement of various properties and phenomena associated, such as physical transitions (glass transition, melting and crystallization, polymorphic transitions, etc.).