UNE EN ISO 11409:1999
PLASTICS - PHENOLIC RESINS - DETERMINATION OF HEATS AND TEMPERATURES OF REACTION BY DIFFERENTIAL SCANNING CALORIMETRY (ISO 11409:1993)
Plásticos. Resinas fenólicas. Determinación de los calores y temperaturas de reacción por calorimetría diferencial de barrido. (ISO 11409:1993).
Format
Availability
Price and currency
English PDF
Immediate download
90.07 USD
English Hardcopy
In stock
90.07 USD
Spanish PDF
Immediate download
75.06 USD
Spanish Hardcopy
In stock
75.06 USD
Standard number: | UNE EN ISO 11409:1999 |
Pages: | 14 |
Released: | 1999-09-21 |
Status: | Standard |
Pages (English): | 14 |
Pages (Spanish): | 14 |
DESCRIPTION
This standard UNE EN ISO 11409:1999 PLASTICS - PHENOLIC RESINS - DETERMINATION OF HEATS AND TEMPERATURES OF REACTION BY DIFFERENTIAL SCANNING CALORIMETRY (ISO 11409:1993) is classified in these ICS categories:
- 83.080.10