ASTM A0608_A0608M-20

Standard Specification for Centrifugally Cast Iron-Chromium-Nickel High-Alloy Tubing for Pressure Application at High Temperatures

Format
Availability
Price and currency
English PDF Redline
Immediate download
68.48 USD
PDF
Immediate download
57.78 USD
Hardcopy
In stock
57.78 USD
Language:English
Released:2020-06-02
Pages:6
Standards number:ASTM A0608_A0608M-20
Standard number:A0608_A0608M-20
Released:01.05.2020
Status:Active
Pages:6
Section:01.02
Keywords:alloy; centrifugal casting; high temperatures; pressure containing parts; steel tube; temperature service applications;
DESCRIPTION

1.1 This specification covers iron-chromium-nickel, high-alloy tubes made by the centrifugal casting process intended for use under pressure at high temperatures.

1.2 The grades of high alloys detailed in Table 1 are intended for applications requiring strength and resistance to corrosion and scaling at high temperatures.

1.3 Optional Supplementary Requirements S1 to S11 are provided; these call for additional tests to be made if desired.

1.4 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard.

1.4.1 Within the text, the SI units are shown in brackets.

1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.