Main page>ASTM Standards>77>77.140>77.140.60>ASTM A0638_A0638M-23 - Standard Specification for Precipitation Hardening Iron Base Superalloy Bars, Forgings, and Forging Stock for High-Temperature Service
Released: 01.05.2023

ASTM A0638_A0638M-23

Standard Specification for Precipitation Hardening Iron Base Superalloy Bars, Forgings, and Forging Stock for High-Temperature Service

Format
Availability
Price and currency
English Secure PDF Redline
Immediate download
Non-printable
244.71 USD
English Secure PDF
Immediate download
Non-printable
221.18 USD
Standard number:ASTM A0638_A0638M-23
Released:01.05.2023
Status:Active
Pages:3
Section:01.03
Keywords:precipitation hardening superalloy steel; superalloy steel bars; superalloy steel billets; superalloy steel forgings; temperature service applications (high);
ASTM number:ASTM A638/A638M
Supersedes:A0638_A0638M-20

This specification covers hot-finished or cold-finished precipitation hardening iron base superalloy bars, forgings, and forging stock for high-temperature service. The mechanical properties of these alloys are developed by suitable solution treating and precipitation hardening treatments. Two grades of iron base alloy are covered; Grade 660 and Grade 662 (bars and forgings). The material shall meet the requirements as to stress rupture properties specified. The material shall conform to the chemical, mechanical, and metallurgical properties requirements specified.

DESCRIPTION

1.1 This specification2 covers hot-finished or cold-finished precipitation hardening iron base superalloy bars, forgings, and forging stock for high-temperature service. The mechanical properties of these alloys are developed by suitable solution treating and precipitation hardening treatments.

1.2 Two grades of iron base alloy are covered. Selection will depend upon design, service conditions, mechanical properties, and elevated temperature characteristics.

1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. SI units are shown in brackets. The values stated in each system are not necessarily exact equivalents; therefore, to ensure conformance with the standard, each system shall be used independently of the other, and values from the two systems shall not be combined.

1.4 Unless the order specifies an “M” designation, the material shall be furnished to inch-pound units.

1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Related products
English Secure PDF Redline
Immediate download
Non-printable
244.71 USD
English Secure PDF
Immediate download
Non-printable
221.18 USD
English Secure PDF Redline
Immediate download
Non-printable
244.71 USD
English Secure PDF
Immediate download
Non-printable
221.18 USD
English Secure PDF Redline
Immediate download
Non-printable
244.71 USD
English Secure PDF
Immediate download
Non-printable
221.18 USD
English Secure PDF Redline
Immediate download
Non-printable
244.71 USD
English Secure PDF
Immediate download
Non-printable
221.18 USD