Using Artificial Intelligence (AI) on standards and related intellectual property is strongly prohibited. In the event of a violation, your access to the standards will be revoked.

PRICES include / exclude VAT
Main page>ASTM Standards>71>71.040>71.040.50>ASTM E1829-14R26 - Standard Guide for Handling Specimens Prior to Surface Analysis
Released: 01.09.2026

ASTM E1829-14R26

Standard Guide for Handling Specimens Prior to Surface Analysis

Format
Availability
Price and currency
English Secure PDF
Immediate download
Non-printable
221.18 USD
Standard number:ASTM E1829-14R26
Released:01.09.2026
Status:Active
Pages:5
Section:03.06
Keywords:Auger electron spectroscopy; secondary ion mass spectrometry; specimen handling; surface analysis; X-ray photoelectron spectroscopy;
ASTM number:ASTM E1829
Supersedes:E1829-14R20
DESCRIPTION

1.1 This guide covers specimen handling and preparation prior to surface analysis and applies to the following surface analysis disciplines:

1.1.1 Auger electron spectroscopy (AES),

1.1.2 X-ray photoelectron spectroscopy (XPS or ESCA), and

1.1.3 Secondary ion mass spectrometry (SIMS).

1.1.4 Although primarily written for AES, XPS, and SIMS, these methods may also apply to many surface-sensitive analysis methods, such as ion scattering spectrometry, low-energy electron diffraction, and electron energy loss spectroscopy, where specimen handling can influence surface-sensitive measurements.

1.2 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.3 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.