Using Artificial Intelligence (AI) on standards and related intellectual property is strongly prohibited. In the event of a violation, your access to the standards will be revoked.

PRICES include / exclude VAT
Main page>BSI Standards >31 ELECTRONICS>31.180 Printed circuits and boards>BS EN 61249-2-30:2013 Materials for printed boards and other interconnecting structures Reinforced base materials clad and unclad. Non-halogenated epoxide modified cyanate ester woven glass laminate of defined flammability (vertical burning test), copper-clad
immediate downloadReleased: 2013-04-30
BS EN 61249-2-30:2013 Materials for printed boards and other interconnecting structures Reinforced base materials clad and unclad. Non-halogenated epoxide modified cyanate ester woven glass laminate of defined flammability (vertical burning test), copper-clad

BS EN 61249-2-30:2013

Materials for printed boards and other interconnecting structures Reinforced base materials clad and unclad. Non-halogenated epoxide modified cyanate ester woven glass laminate of defined flammability (vertical burning test), copper-clad

Format
Availability
Price and currency
English Secure PDF
Immediate download
Printable - You are authorized to print 1 copy
271.44 EUR
English Hardcopy
In stock
271.44 EUR
Standard number:BS EN 61249-2-30:2013
Pages:26
Released:2013-04-30
ISBN:978 0 580 69352 6
Status:Standard
DESCRIPTION

BS EN 61249-2-30:2013


This standard BS EN 61249-2-30:2013 Materials for printed boards and other interconnecting structures is classified in these ICS categories:
  • 31.180 Printed circuits and boards

This part of IEC 61249 gives requirements for properties of non-halogenated epoxide modified cyanate ester woven glass laminate of defined flammability (vertical burning test), copper-clad in thicknesses of 0,03 mm up to 1,60 mm. The flammability rating is achieved through the use of non-halogenated inorganic and/or organic compounds acting as fire retardants. These fire retardants are contained as part of polymeric structure or in addition to it. The glass transition temperature is defined to be 160 °C minimum.

Some property requirements may have several classes of performance. The class desired should be specified on the purchase order, otherwise the default class of material may be supplied.


Other parts of the standard
English Secure PDF
Immediate download
Printable - You are authorized to print 1 copy
23.40 EUR
English Hardcopy
In stock
23.40 EUR
English Secure PDF
Immediate download
Printable - You are authorized to print 1 copy
23.40 EUR
English Hardcopy
In stock
23.40 EUR
English Secure PDF
Immediate download
Printable - You are authorized to print 1 copy
271.44 EUR
English Hardcopy
In stock
271.44 EUR