PRICES include / exclude VAT
Main page>BSI Standards >81 GLASS AND CERAMICS INDUSTRIES>81.060 Ceramics>81.060.30 Advanced ceramics>BS EN 843-6:2009 Advanced technical ceramics. Mechanical properties of monolithic ceramics at room temperature Guidance for fractographic investigation
immediate downloadReleased: 2010-01-31
BS EN 843-6:2009 Advanced technical ceramics. Mechanical properties of monolithic ceramics at room temperature Guidance for fractographic investigation

BS EN 843-6:2009

Advanced technical ceramics. Mechanical properties of monolithic ceramics at room temperature Guidance for fractographic investigation

Format
Availability
Price and currency
English Secure PDF
Immediate download
Printable - You are authorized to print 1 copy
414.00 USD
English Hardcopy
In stock
414.00 USD
Standard number:BS EN 843-6:2009
Pages:48
Released:2010-01-31
ISBN:978 0 580 63845 9
Status:Standard
DESCRIPTION

BS EN 843-6:2009


This standard BS EN 843-6:2009 Advanced technical ceramics. Mechanical properties of monolithic ceramics at room temperature is classified in these ICS categories:
  • 81.060.30 Advanced ceramics