Main page>BSI Standards >83 RUBBER AND PLASTICS INDUSTRIES>83.080 Plastics>83.080.01 Plastics in general>BS EN ISO 11357-5:2025 - TC Tracked Changes. Plastics. Differential scanning calorimetry (DSC) Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion
immediate downloadReleased: 2025-06-04
BS EN ISO 11357-5:2025 - TC Tracked Changes. Plastics. Differential scanning calorimetry (DSC) Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion

BS EN ISO 11357-5:2025 - TC

Tracked Changes. Plastics. Differential scanning calorimetry (DSC) Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion

Format
Availability
Price and currency
English Secure PDF
Immediate download
Printable - You are authorized to print 1 copy
322.09 USD
English Hardcopy
In stock
322.09 USD
Standard number:BS EN ISO 11357-5:2025 - TC
Pages:40
Released:2025-06-04
ISBN:978 0 539 37319 6
Status:Tracked Changes
DESCRIPTION

BS EN ISO 11357-5:2025 - TC


This standard BS EN ISO 11357-5:2025 - TC Tracked Changes. Plastics. Differential scanning calorimetry (DSC) is classified in these ICS categories:
  • 83.080.01 Plastics in general
This document specifies a method for the determination of reaction temperatures and times, enthalpies of reaction, and degrees of conversion using conventional differential scanning calorimetry (DSC) as specified in ISO 11357-1. The method applies to monomers, prepolymers, and polymers in the solid or liquid state. The material can contain fillers and/or initiators in the solid or liquid state. This document is not applicable to fast DSC as specified in ISO 23976.[1]