BS EN ISO 15614-3:2008 Specification and qualification of welding procedures for metallic materials. Welding procedure test Fusion welding of non-alloyed and low-alloyed cast irons

BS EN ISO 15614-3:2008

Specification and qualification of welding procedures for metallic materials. Welding procedure test Fusion welding of non-alloyed and low-alloyed cast irons

Format
Availability
Price and currency
English Secure PDF
Immediate download
Printable - You are authorized to print 1 copy
319.34 USD
English Hardcopy
In stock
319.34 USD
Standard number:BS EN ISO 15614-3:2008
Pages:26
Released:2008-07-31
ISBN:978 0 580 54475 0
Status:Standard
DESCRIPTION

BS EN ISO 15614-3:2008


This standard BS EN ISO 15614-3:2008 Specification and qualification of welding procedures for metallic materials. Welding procedure test is classified in these ICS categories:
  • 25.160.10 Welding processes

This part of ISO 15614 specifies how a preliminary welding procedure specification (pWPS) for production and repair welding of non-alloyed and low-alloyed cast irons is qualified by fusion welding procedure tests.

This part of ISO 15614 defines the conditions for execution of the welding procedure tests and the range of qualification for welding procedures for all practical welding operations within the range of a defined list of variables.

This part of ISO 15614 is applicable to all new welding procedures. However, it does not invalidate previous welding procedure tests made to former national standards or specifications. Where additional tests have to be carried out to make the qualification technically equivalent, it is only necessary to do the additional tests on a test piece made in accordance with this part of ISO 15614.

Additional tests may be required by application standards.

This part of ISO 15614 is applicable to welding non-alloyed and low-alloyed grey cast iron castings according to: EN 1561; EN 1562; EN 1563; and EN 1564.

The principles of this part of ISO 15614 are also applicable for welding cast iron to steel or to other unalloyed and low-alloyed cast iron materials.