Homepage>BS Standards>81 GLASS AND CERAMICS INDUSTRIES>81.060 Ceramics>81.060.30 Advanced ceramics>BS ISO 19604:2018 Fine ceramics (advanced ceramics, advanced technical ceramics). Mechanical properties of ceramic composites at high temperature. Determination of stress-rupture time diagram under constant tensile loading
immediate downloadReleased: 2018-05-01
BS ISO 19604:2018 Fine ceramics (advanced ceramics, advanced technical ceramics). Mechanical properties of ceramic composites at high temperature. Determination of stress-rupture time diagram under constant tensile loading

BS ISO 19604:2018

Fine ceramics (advanced ceramics, advanced technical ceramics). Mechanical properties of ceramic composites at high temperature. Determination of stress-rupture time diagram under constant tensile loading

Format
Availability
Price and currency
English Secure PDF
Immediate download
270.40 USD
You can read the standard for 1 hour. More information in the category: E-reading
Reading the standard
for 1 hour
27.04 USD
You can read the standard for 24 hours. More information in the category: E-reading
Reading the standard
for 24 hours
81.12 USD
English Hardcopy
In stock
270.40 USD
Standard number:BS ISO 19604:2018
Pages:28
Released:2018-05-01
ISBN:978 0 580 86684 5
Status:Standard
DESCRIPTION

BS ISO 19604:2018


This standard BS ISO 19604:2018 Fine ceramics (advanced ceramics, advanced technical ceramics). Mechanical properties of ceramic composites at high temperature. Determination of stress-rupture time diagram under constant tensile loading is classified in these ICS categories:
  • 81.060.30 Advanced ceramics

This document specifies the conditions for determination of the stress-rupture time diagram of continuous fibre-reinforced ceramic matrix composites (including carbon fibre-reinforced carbon matrix composite) at high temperature in air, vacuum and inert gas atmospheres under constant tensile loading.

This document applies to all ceramic matrix composites with continuous fibre reinforcement: unidirectional (1D), bidirectional (2D) and tridirectional (xD, with 2 < x ≤ 3), loaded along one principal axis of reinforcement.

NOTE 1 In most cases, ceramic matrix composites to be used at high temperature in air are coated with an antioxidation coating.

NOTE 2 Since the main purpose of the test is to obtain the stress-rupture time data, the deformation measurement is not mandatory.