PRICES include / exclude VAT
Sponsored link
immediate downloadReleased: 2019-05-03
BS ISO 21746:2019
Composites and metal assemblies. Galvanic corrosion tests of carbon fibre reinforced plastics (CFRPs) related bonded or fastened structures in artificial atmospheres. Salt spray tests
Format
Availability
Price and currency
English Secure PDF
Immediate download
270.40 USD
You can read the standard for 1 hour. More information in the category: E-reading
Reading the standardfor 1 hour
27.04 USD
You can read the standard for 24 hours. More information in the category: E-reading
Reading the standardfor 24 hours
81.12 USD
English Hardcopy
In stock
270.40 USD
Standard number: | BS ISO 21746:2019 |
Pages: | 28 |
Released: | 2019-05-03 |
ISBN: | 978 0 580 95914 1 |
Status: | Standard |
DESCRIPTION
BS ISO 21746:2019
This standard BS ISO 21746:2019 Composites and metal assemblies. Galvanic corrosion tests of carbon fibre reinforced plastics (CFRPs) related bonded or fastened structures in artificial atmospheres. Salt spray tests is classified in these ICS categories:
- 83.120 Reinforced plastics
This document specifies the apparatus, the reagents and the procedure to be used in conducting the neutral salt spray (NSS), acetic acid salt spray (AASS) and copper-accelerated acetic acid salt spray (CASS) tests for assessment of the galvanic corrosion resistance of joints and bonded structures between carbon fibre reinforced plastics (CFRPs) and metallic materials, with or without permanent or temporary insulation for the galvanic current.