CSN EN ISO 11357-3 - Plastics - Differential scanning calorimetry (DSC) - Part 3: Determination of temperature and enthalpy of melting and crystallization

CSN EN ISO 11357-3

Plastics - Differential scanning calorimetry (DSC) - Part 3: Determination of temperature and enthalpy of melting and crystallization

Format
Availability
Price and currency
English Hardcopy
In stock
82.35 USD
FREE Shipping
Number of Standard:CSN EN ISO 11357-3
Category:640748
Pages:20
Released:01.11.2025
Catalog number:522145
DESCRIPTION

CSN EN ISO 11357-3

CSN EN ISO 11357-3 This document specifies a method for the determination of the temperatures and enthalpies of melting and crystallization of crystalline or partially crystalline plastics using conventional DSC as specified in ISO 11357-1. This document is not applicable to fast DSC as specified in ISO 23976.
Original English text of CSN EN Standard.