ISO 11970:2025 - Specification and qualification of welding procedures for production welding of steel and nickel-base castings

ISO 11970:2025

ISO 11970:2025 - Specification and qualification of welding procedures for production welding of steel and nickel-base castings

Format
Availability
Price and currency
English PDF
Immediate download
Printable
127.06 USD
English Hardcopy
in stock
127.06 USD
French PDF
Immediate download
Printable
127.06 USD
French Hardcopy
in stock
127.06 USD
Standard´s number:ISO 11970:2025
Edition:3
Released:2025-11-14
Pages (English):17
Pages (French):17
DESCRIPTION

ISO 11970:2025

This document specifies how a welding procedure specification (WPS) for production welding of steel castings is qualified. Tests are intended to be carried out in accordance with this document, unless additional tests are specified by the purchaser or by agreement between the contracting parties.

This document defines the conditions for the execution of welding procedure qualification tests and the limits of validity of a qualified welding procedure for all practical welding operations within the range of essential variables.

This document applies to the arc welding of steel castings. The principles of this document can be applied to other fusion welding processes subject to agreement between the contracting parties.