Main page>ISO Standards>ISO 16433:2006 - Resistance welding — Procedure for seam welding of uncoated and coated low carbon steels
immediate downloadReleased: 2006-03-29
ISO 16433:2006 - Resistance welding — Procedure for seam welding of uncoated and coated low carbon steels

ISO 16433:2006

ISO 16433:2006 - Resistance welding — Procedure for seam welding of uncoated and coated low carbon steels

Format
Availability
Price and currency
English PDF
Immediate download
Printable
145.80 EUR
English Hardcopy
In stock
145.80 EUR
French PDF
Immediate download
Printable
145.80 EUR
French Hardcopy
In stock
145.80 EUR
Standard´s number:ISO 16433:2006
Edition:1
Released:2006-03-29
Pages (English):20
Pages (French):22
DESCRIPTION

ISO 16433:2006

ISO16433:2006 specifies requirements for resistance seam welding in the fabrication of assemblies of uncoated and metallic coated low carbon steel comprising two sheets of metal, where the maximum single sheet thickness of components to be welded is within the range 0,4 mm to 3 mm for the following materials:

  • uncoated steels;
  • hot-dip zinc or iron-zinc alloy (galvannealed) coated steel;
  • electrolytic zinc, zinc-iron, or zinc-nickel coated steel;
  • aluminium coated steel;
  • zinc-aluminium coated steel.