Using Artificial Intelligence (AI) on standards and related intellectual property is strongly prohibited. In the event of a violation, your access to the standards will be revoked.

PRICES include / exclude VAT
Main page>ISO Standards>ISO 204:2023 - Metallic materials — Uniaxial creep testing in tension — Method of test
immediate downloadReleased: 2023-07-25
ISO 204:2023 - Metallic materials — Uniaxial creep testing in tension — Method of test

ISO 204:2023

ISO 204:2023 - Metallic materials — Uniaxial creep testing in tension — Method of test

Format
Availability
Price and currency
English PDF
Immediate download
Printable
229.98 USD
English Hardcopy
In stock
229.98 USD
French PDF
Immediate download
Printable
229.98 USD
French Hardcopy
In stock
229.98 USD
Standard´s number:ISO 204:2023
Edition:4
Released:2023-07-25
Pages (English):48
Pages (French):50
DESCRIPTION

ISO 204:2023

This document specifies the methods for:

a)    uninterrupted creep tests with continuous monitoring of extension;

b)    interrupted creep tests with periodic measurement of elongation;

c)    stress rupture tests where normally only the time to fracture is measured;

d)    a test to verify that a predetermined time can be exceeded under a given force, with the elongation or extension not necessarily being reported.

NOTE       A creep test can be continued until fracture has occurred or it can be stopped before fracture.