Main page>ISO Standards>ISO 6957:1988 - Copper alloys — Ammonia test for stress corrosion resistance
immediate downloadReleased: 1988-09-15
ISO 6957:1988 - Copper alloys — Ammonia test for stress corrosion resistance

ISO 6957:1988

ISO 6957:1988 - Copper alloys — Ammonia test for stress corrosion resistance

Format
Availability
Price and currency
English PDF
Immediate download
Printable
55.91 USD
English Hardcopy
In stock
55.91 USD
French PDF
Immediate download
Printable
55.91 USD
French Hardcopy
In stock
55.91 USD
Standard´s number:ISO 6957:1988
Edition:1
Released:1988-09-15
Pages (English):3
Pages (French):3
DESCRIPTION

ISO 6957:1988

Specifies a test, using an ammoniacal atmosphere, for the detection of applied or residual stresses which can cause failure of the material in service or storage through stress corrosion cracking. The severity of the method can be regulated by changing the pH value. In an informative annex, recommendations are given for the choice of pH-values.