Main page>ISO Standards>ISO 7500-2:2006 - Metallic materials — Verification of static uniaxial testing machines — Part 2: Tension creep testing machines — Verification of the applied force
immediate downloadReleased: 2006-12-05
ISO 7500-2:2006 - Metallic materials — Verification of static uniaxial testing machines — Part 2: Tension creep testing machines — Verification of the applied force

ISO 7500-2:2006

ISO 7500-2:2006 - Metallic materials — Verification of static uniaxial testing machines — Part 2: Tension creep testing machines — Verification of the applied force

Format
Availability
Price and currency
English PDF
Immediate download
Printable
127.06 USD
English Hardcopy
In stock
127.06 USD
French PDF
Immediate download
Printable
127.06 USD
French Hardcopy
In stock
127.06 USD
Standard´s number:ISO 7500-2:2006
Edition:2
Released:2006-12-05
Pages (English):17
Pages (French):17
DESCRIPTION

ISO 7500-2:2006

ISO 7500-2:2006 specifies the verification of testing machines used for uniaxial creep testing in tension in accordance with ISO 204.

The verification consists of

  • a general inspection of the testing machine, and
  • a verification of the force applied by the testing machine.

ISO 7500-2:2006 applies to dead-weight machines, lever-type creep testing machines and direct-spring-loading machines.

Machines with a force-measuring system should be verified in accordance with ISO 7500-1.