Main page>ISO Standards>ISO 7539-8:2000 - Corrosion of metals and alloys — Stress corrosion testing — Part 8: Preparation and use of specimens to evaluate weldments
immediate downloadReleased: 2000-06-29
ISO 7539-8:2000
ISO 7539-8:2000 - Corrosion of metals and alloys — Stress corrosion testing — Part 8: Preparation and use of specimens to evaluate weldments
Format
Availability
Price and currency
English PDF
Immediate download
Printable
108.00 EUR
English Hardcopy
In stock
108.00 EUR
French PDF
Immediate download
Printable
108.00 EUR
French Hardcopy
In stock
108.00 EUR
Standard´s number:
ISO 7539-8:2000
Edition:
1
Released:
2000-06-29
Pages (English):
18
Pages (French):
19
DESCRIPTION
ISO 7539-8:2000
La présente partie de l'ISO 7539 traite des modes opératoires existants pour les essais de corrosion sous contrainte . des éprouvettes soudées et étudie les facteurs supplémentaires à prendre en compte lorsqu'on effectue des essais sur des éprouvettes soudées. La présente partie de l'ISO 7539 donne notamment des recommandations concernant le choix des éprouvettes et fournit des méthodes d'essai pour déterminer la résistance d'un métal à la corrosion sous contrainte, quand il est soudé. Le terme «métal» utilisé dans la présente partie de l'ISO 7539 inclut également les alliages.