Main page>UNE standards>UNE EN 12814-3:2014 - Testing of welded joints in thermoplastics semi-finished products - Part 3: Tensile creep test
in stockReleased: 2014-10-15
UNE EN 12814-3:2014 - Testing of welded joints in thermoplastics semi-finished products - Part 3: Tensile creep test

UNE EN 12814-3:2014

Testing of welded joints in thermoplastics semi-finished products - Part 3: Tensile creep test

Ensayo de uniones soldadas en productos termoplásticos semiacabados. Parte 3: Ensayo de fluencia en tracción.

Format
Availability
Price and currency
English PDF
Immediate download
Printable
81.40 EUR
English Hardcopy
In stock
81.40 EUR
Spanish PDF
Immediate download
Printable
81.40 EUR
Spanish Hardcopy
In stock
81.40 EUR
Standard number:UNE EN 12814-3:2014
Pages:28
Released:2014-10-15
Status:Standard
DESCRIPTION

UNE EN 12814-3:2014

Esta norma europea especifica las dimensiones, el método de muestreo y la preparación de probetas y condiciones para llevar a cabo el ensayo de fluencia en tracción perpendicularmente a la soldadura para determinar el factor de soldadura en tracción a largo plazo. Puede emplearse un ensayo de fluencia junto con otros ensayos (por ejemplo, ensayo de curvatura, ensayo de tracción, examen macrográfico...) para evaluar el comportamiento de los conjuntos soldados fabricados a partir de materiales termoplásticos. Este ensayo se aplica a conjuntos soldados de materiales termoplásticos, con o sin relleno, como tuberías y accesorios, láminas, placas, perfiles, nunca reforzados, independientemente del proceso de soldadura utilizado.

Other parts of the standard
English PDF
Immediate download
Printable
75.90 EUR
English Hardcopy
In stock
75.90 EUR
Spanish PDF
Immediate download
Printable
75.90 EUR
Spanish Hardcopy
In stock
75.90 EUR
English PDF
Immediate download
Printable
64.90 EUR
English Hardcopy
In stock
64.90 EUR
Spanish PDF
Immediate download
Printable
64.90 EUR
Spanish Hardcopy
In stock
64.90 EUR
English PDF
Immediate download
Printable
71.50 EUR
English Hardcopy
In stock
71.50 EUR
Spanish PDF
Immediate download
Printable
71.50 EUR
Spanish Hardcopy
In stock
71.50 EUR
English PDF
Immediate download
Printable
67.10 EUR
English Hardcopy
In stock
67.10 EUR
Spanish PDF
Immediate download
Printable
67.10 EUR
Spanish Hardcopy
In stock
67.10 EUR
English PDF
Immediate download
Printable
79.20 EUR
English Hardcopy
In stock
79.20 EUR
Spanish PDF
Immediate download
Printable
79.20 EUR
Spanish Hardcopy
In stock
79.20 EUR
English PDF
Immediate download
Printable
56.10 EUR
English Hardcopy
In stock
56.10 EUR
Spanish PDF
Immediate download
Printable
56.10 EUR
Spanish Hardcopy
In stock
56.10 EUR
English PDF
Immediate download
Printable
71.50 EUR
English Hardcopy
In stock
71.50 EUR
Spanish PDF
Immediate download
Printable
71.50 EUR
Spanish Hardcopy
In stock
71.50 EUR