Main page>UNE standards>UNE EN 6041:2018 - Aerospace series - Non-metallic materials - Test method - Analysis of non-metallic materials (uncured) by Differential Scanning Calorimetry (DSC) (Endorsed by Asociación Española de Normalización in March of 2018.)
in stockReleased: 2018-03-01
UNE EN 6041:2018 - Aerospace series - Non-metallic materials - Test method - Analysis of non-metallic materials (uncured) by Differential Scanning Calorimetry (DSC) (Endorsed by Asociación Española de Normalización in March of 2018.)

UNE EN 6041:2018

Aerospace series - Non-metallic materials - Test method - Analysis of non-metallic materials (uncured) by Differential Scanning Calorimetry (DSC) (Endorsed by Asociación Española de Normalización in March of 2018.)

Material aeroespacial. Materiales no metálicos. Método de ensayo. Análisis de materiales no metálicos (sin curar) por calorímetro diferencial (DSC). (Ratificada por la Asociación Española de Normalización en marzo de 2018.)

Format
Availability
Price and currency
English PDF
Immediate download
Printable
76.35 USD
English Hardcopy
In stock
76.35 USD
Standard number:UNE EN 6041:2018
Pages:15
Released:2018-03-01
Status:Standard
DESCRIPTION

UNE EN 6041:2018

This test method defines the procedure for the determination of the curing-characteristic and glass transition temperature of non-metallic materials (e.g. preimpregnated and neat resin systems, adhesives) for aerospace use by Differential Scanning Calorimetry (DSC). The results obtained by this method may be useful for: - derivation of the optimum cure cycle (only together with other test methods e.g. Tg determination) - assessment of the condition of the resin - assessment of the ageing behavior of the resin This European Standard does not give any directions necessary to meet the health and safety requirements. It is the responsibility of the user of this European Standard to adopt appropriate health and safety precautions.