UNE EN ISO 11357-3:2026 - Plastics - Differential scanning calorimetry (DSC) - Part 3: Determination of temperature and enthalpy of melting and crystallization (ISO 11357-3:2025)

UNE EN ISO 11357-3:2026

Plastics - Differential scanning calorimetry (DSC) - Part 3: Determination of temperature and enthalpy of melting and crystallization (ISO 11357-3:2025)

Plásticos. Calorimetría diferencial de barrido (DSC). Parte 3: Determinación de la temperatura y de la entalpía de fusión y de cristalización. (ISO 11357-3:2025).

Format
Availability
Price and currency
English PDF
Immediate download
Printable
78.94 USD
English Hardcopy
In stock
78.94 USD
Spanish PDF
Immediate download
Printable
78.94 USD
Spanish Hardcopy
In stock
78.94 USD
Standard number:UNE EN ISO 11357-3:2026
Pages:14
Released:2026-02-25
Status:Standard
DESCRIPTION

UNE EN ISO 11357-3:2026

This document specifies a method for the determination of the temperatures and enthalpies of melting and crystallization of crystalline or partially crystalline plastics using conventional DSC as specified in ISO 11357-1. This document is not applicable to fast DSC as specified in ISO 23976.