PRICES include / exclude VAT
Main page>UNE standards>UNE EN ISO 14373:2024 - Resistance welding - Procedure for spot welding of uncoated and coated low carbon steels (ISO 14373:2024)
in stockReleased: 2024-10-02
UNE EN ISO 14373:2024 - Resistance welding - Procedure for spot welding of uncoated and coated low carbon steels (ISO 14373:2024)

UNE EN ISO 14373:2024

Resistance welding - Procedure for spot welding of uncoated and coated low carbon steels (ISO 14373:2024)

Soldeo por resistencia. Procedimiento para el soldeo por puntos de aceros bajos en carbono recubiertos y no recubiertos. (ISO 14373:2024).

Format
Availability
Price and currency
English PDF
Immediate download
Printable
95.76 USD
English Hardcopy
In stock
95.76 USD
Spanish PDF
Immediate download
Printable
95.76 USD
Spanish Hardcopy
In stock
95.76 USD
Standard number:UNE EN ISO 14373:2024
Pages:23
Released:2024-10-02
Status:Standard
Pages (Spanish):26
DESCRIPTION

UNE EN ISO 14373:2024

This document specifies requirements for resistance spot welding in the fabrication of assemblies of uncoated, and metallic coated or weldable non-metallic coated low carbon steel, comprising two or three sheets of metal, where the maximum single sheet thickness of components to be welded is within the range 0,4 mm to 3 mm. This document is applicable to welding of sheets of the same or unequal thickness, where the thickness ratio is less than or equal to 3:1. It applies to the welding of three sheets, where the total thickness is less than or equal to 9 mm. Welding with the following types of equipment is within the scope of this document: a) pedestal welding equipment; b) portable welding guns; c) automatic welding equipment where the components are fed by robots or automatic feeding equipment; d) multi-spot welding machine; e) robotic welding machine. Information on appropriate welding equipment is given in Annex A, and information on spot welding conditions is given in Annex B. This information is provided for guidance only. Depending on the service conditions of the fabrication, the type of welding equipment, the characteristics of the secondary circuit, electrode force actuation system,, the electrode material, and the shape, it is possible that certain modifications are necessary. In such cases, further information can be obtained from the relevant application standard, where one exists.