UNE EN ISO 18785-4:2021 - Friction stir spot welding - Aluminium - Part 4: Specification and qualification of welding procedures (ISO 18785-4:2018)

UNE EN ISO 18785-4:2021

Friction stir spot welding - Aluminium - Part 4: Specification and qualification of welding procedures (ISO 18785-4:2018)

Soldadura por fricción y agitación por puntos. Aluminio. Parte 4: Especificación y cualificación de los procedimientos de soldadura. (ISO 18785-4:2018).

Format
Availability
Price and currency
English PDF
Immediate download
Printable
91.88 USD
English Hardcopy
In stock
91.88 USD
Spanish PDF
Immediate download
Printable
91.88 USD
Spanish Hardcopy
In stock
91.88 USD
Standard number:UNE EN ISO 18785-4:2021
Pages:22
Released:2021-07-28
Status:Standard
Pages (Spanish):23
DESCRIPTION

UNE EN ISO 18785-4:2021

This document specifies the requirements for the content of welding procedure specifications for the Friction Stir Spot welding (FSSW) of aluminium. In this document, the term "aluminium" refers to aluminium and its alloys