Using Artificial Intelligence (AI) on standards and related intellectual property is strongly prohibited. In the event of a violation, your access to the standards will be revoked.
Main page>UNE standards>UNE EN ISO 204:2024 - Metallic materials - Uniaxial creep testing in tension - Method of test (ISO 204:2023)
in stockReleased: 2024-04-10
UNE EN ISO 204:2024
Metallic materials - Uniaxial creep testing in tension - Method of test (ISO 204:2023)
Materiales metálicos. Ensayo de fluencia uniaxial en tracción. Método de ensayo. (ISO 204:2023).
Format
Availability
Price and currency
English PDF
Immediate download
Printable
152.71 USD
English Hardcopy
In stock
152.71 USD
Spanish PDF
Immediate download
Printable
152.71 USD
Spanish Hardcopy
In stock
152.71 USD
Standard number:
UNE EN ISO 204:2024
Pages:
58
Released:
2024-04-10
Status:
Standard
Pages (Spanish):
67
DESCRIPTION
UNE EN ISO 204:2024
This document specifies the methods for a) uninterrupted creep tests with continuous monitoring of extension, b) interrupted creep tests with periodic measurement of elongation, c) stress rupture tests where normally only the time to fracture is measured, d) a test to verify that a predetermined time can be exceeded under a given force, with the elongation or extension not necessarily being reported. NOTE A creep test can be continued until fracture has occurred or it can be stopped before fracture.