ASTM G0047-26
Standard Test Method for Determining Susceptibility to Stress-Corrosion Cracking of 2XXX and 7XXX Aluminum Alloy Products
| Standard number: | ASTM G0047-26 |
| Released: | 01.05.2026 |
| Status: | Active |
| Pages: | 7 |
| Section: | 03.02 |
| Keywords: | accelerated testing; aluminum alloys; corrosion; heat-treatable aluminum alloys; stress-corrosion cracking; tension testing; |
| ASTM number: | ASTM G47 |
| Supersedes: | G0047-22 |
1.1 This test method covers a uniform procedure for characterizing the resistance to stress-corrosion cracking (SCC) of high-strength aluminum alloy wrought products for the guidance of those who perform stress-corrosion tests, for those who prepare stress-corrosion specifications, and for materials engineers.
1.2 This test method covers method of sampling, type of specimen, specimen preparation, test environment, and method of exposure for determining the susceptibility to SCC of 2XXX (with 1.8 % to 7.0 % copper) and 7XXX (with 0.4 % to 2.8 % copper) aluminum alloy products, particularly when stressed in the short-transverse direction relative to the grain structure.
1.3 The values stated in SI units are to be regarded as standard. The values given in parentheses after SI units are provided for information only and are not considered standard.
1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.
1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.
Standard Terminology Relating to Methods of Mechanical Testing
Standard Terminology Relating to Metallography
Standard Test Methods and Definitions for Mechanical Testing of Steel Products
Standard Test Methods for Rockwell Hardness of Metallic Materials