Using Artificial Intelligence (AI) on standards and related intellectual property is strongly prohibited. In the event of a violation, your access to the standards will be revoked.

PRICES include / exclude VAT
Main page>ASTM Standards>77>77.120>77.120.10>ASTM G0064-99R21 - Standard Classification of Resistance to Stress-Corrosion Cracking of Heat-Treatable Aluminum Alloys
Released: 01.08.2021

ASTM G0064-99R21

Standard Classification of Resistance to Stress-Corrosion Cracking of Heat-Treatable Aluminum Alloys

Format
Availability
Price and currency
English Secure PDF
Immediate download
Non-printable
221.18 USD
Standard number:ASTM G0064-99R21
Released:01.08.2021
Status:Active
Pages:4
Section:03.02
Keywords:alphabetical stress–corrosion ratings; heat–treatable aluminum alloys; laboratory corrosion tests; practical interpretation of ratings; service experience; stress-corrosion tracking;
ASTM number:ASTM G64
Supersedes:G0064-99R13
DESCRIPTION

1.1 This classification covers alphabetical ratings of the relative resistance to SCC of various mill product forms of the wrought 2XXX, 6XXX, and 7XXX series heat-treated aluminum alloys and the procedure for determining the ratings.

1.2 The ratings do not apply to metal in which the metallurgical structure has been altered by welding, forming, or other fabrication processes.

1.3 The values stated in SI units are to be regarded as standard. The values given in parentheses after SI units are provided for information only and are not considered standard.

1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.