PRICES include / exclude VAT
Main page>UNE standards>UNE EN ISO 11357-4:2021 - Plastics - Differential scanning calorimetry (DSC) - Part 4: Determination of specific heat capacity (ISO 11357-4:2021)
in stockReleased: 2021-12-15
UNE EN ISO 11357-4:2021 - Plastics - Differential scanning calorimetry (DSC) - Part 4: Determination of specific heat capacity (ISO 11357-4:2021)

UNE EN ISO 11357-4:2021

Plastics - Differential scanning calorimetry (DSC) - Part 4: Determination of specific heat capacity (ISO 11357-4:2021)

Plásticos. Calorimetría diferencial de barrido (DSC). Parte 4: Determinación de la capacidad calorífica específica. (ISO 11357-4:2021).

Format
Availability
Price and currency
English PDF
Immediate download
Printable
86.71 USD
English Hardcopy
In stock
86.71 USD
Spanish PDF
Immediate download
Printable
86.71 USD
Spanish Hardcopy
In stock
86.71 USD
Standard number:UNE EN ISO 11357-4:2021
Pages:20
Released:2021-12-15
Status:Standard
Pages (Spanish):19
DESCRIPTION

UNE EN ISO 11357-4:2021

This document specifies methods for determining the specific heat capacity of plastics by differential scanning calorimetry.